寻源地 XYD
英标平台标准档案编号:BJT-BS-4174-14-84ED
现行有效

BS 4174-14-2013

BT牙开槽清根半沉头割尾自攻螺钉表14

Type BT slotted truncated raised countersunk head self tapping cutting screw-Table 14

BS 4174-14-2013 BT牙开槽清根半沉头割尾自攻螺钉表14 标准示意图
德标 DIN美标 ASME/ANSI英标 BS
DIN 7516ASME B18.6.4BS 4174-14-2013
螺纹尺寸
d
#2#4#6#8#10#12#14#16
P螺距3224201816141412
k头部厚度 最大值0.0360.0470.0590.070.0810.0920.1070.134
k头部厚度 最小值0.0280.0380.0480.0580.0680.0780.0920.116
dk头部外径 最大值0.1720.2250.2790.3320.3850.4380.5070.635
dk头部外径 最小值0.1470.1950.2440.2920.340.3890.4520.568
d大径 最大值0.0880.1140.1390.1660.1890.2150.2460.315
d大径 最小值0.0840.110.1350.1610.1830.2090.240.308
t槽深0.0370.0480.0590.0710.0820.0940.1090.137
d1max0.0640.0860.1040.1220.1410.1640.1920.244
d1min0.060.0820.0990.1160.1350.1570.1850.236
f参数值0.0250.0330.040.0480.0550.0630.0720.09
nmax0.0310.0390.0480.0540.060.0670.0750.084
nmin0.0230.0310.0390.0450.050.0560.0640.072
该标准(BS 4174-14-2013)暂无直接嵌套的原生规范矩阵表。以下为本标准已归档的核心技术要求:
产品等级A级 (切削自攻级)
推荐性能等级渗碳淬火硬化钢 (表面硬度≥45HRC, 芯部28~38HRC)
表面处理规范镀蓝白锌;镀彩锌;达克罗;黑色磷化;环保三价铬镀锌
主要适配材质碳钢 / 不锈钢 / 合金钢

工程应用场景与制造工艺画像

应用热度指数:75

行业工况与连接用途

所属工业领域:建筑装修/家具
核心连接场景:薄板连接、家具装配、电器外壳固定、石膏板安装
主要功能用途:在预制孔或薄板中自行攻出内螺纹,实现可拆卸连接,适用于金属薄板、塑料及木质件
典型应用节点:

压铸铝合金外壳、厚壁工程塑料、较厚钣金机柜自攻切削紧固,防止滑牙与基体胀裂

生产制造工艺与质量控制

产品等级(精度):A级 (切削自攻级)
常用材料与性能等级:渗碳淬火硬化钢 (表面硬度≥45HRC, 芯部28~38HRC)
对应国际/德标:ASME B18.6.4 (F/T/D/G/BF/BT牙); SAE J933; DIN 7516
推荐表面防腐:镀蓝白锌;镀彩锌;达克罗;黑色磷化;环保三价铬镀锌
全流程工序步骤:

1022A退火线材 → 酸洗轻拉 → 冷镦打头冲十字槽/梅花槽 → 夹尾模冲切排屑切削槽 → 高速搓丝 → 连续网带式渗碳淬火 → 清洗低温回火 → 表面电镀处理 → 恒温去氢退脆烘烤 → 试攻标准钢板破坏力矩检验 → 装盒包装

具备本标准生产与现货能力的源头企业推荐

在全国企业名录中查看更多
暂无直接排产本标准的公开实体工厂

全国对口特色产业集群汇聚海量模具与冷镦机台能力,您可以直接发布针对本标准的采购需求,由源头工厂自主响应报价。

发布本标准采购需求
工程数据声明:上述参数摘录自紧固件相关行业标准文献,用于前期设计选型与通用公差参考。精密装配、特种防腐或大宗采办时,请以官方正版最新标准文件为准。

需要采购或定制 BS 4174-14-2013 (BT牙开槽清根半沉头割尾自攻螺钉表14)?

一键将标准代号、公称尺寸带入发布向导,由系统向全国具备对应模具的实体企业精准撮合。